Abstract

This article presents measurements of the thickness of alcohol-based coatings on sand foundry cores and moulds. These coatings were applied using two methods, the dipping method and the painting method. For the purposes of the study, a zircon alcohol-based coating was prepared with three different levels of nominal viscosity; very thin at 10s, average at 20s, and thick at 30s. The coating was applied to a core made of quartz sand and furan resin. The cores were made of sand with three different grain sizes; dL = 0.22 mm – fine sand, dL = 0.33 mm medium sand, and dL = 0.47 mm coarse sand. In the study, the thickness of the coating obtained to the core was measured immediately after application as well as after drying. Additionally, the extent of penetration into the intergranular spaces of the core matrix was measured. On the basis of this study, the impact of the grain size of the core matrix on the thickness of the coating and its penetration into the core was assessed. The thickness of coatings obtained using different application methods was also assessed.
Go to article

Abstract

The article presents analysis of the influence of ingate size on the Lost Foam casting process. In particular, analysis of simulation tests has been carried out to determine the ingate size influence on the rate of filling of the mould cavity, pressure in the gas gap and size of the gas gap. A specially prepared mathematical model of the process and an original calculation algorithm were used in simulation tests of full-mould casting. The tests have indicated that the increase of the ingate size results in the increase of filling rate and increase of pressure of gases in the gas gap. However, significant influence on mould cavity filling occurs only when the ingate size is less than ~1 cm2. .
Go to article

This page uses 'cookies'. Learn more