Search results

Filters

  • Journals
  • Date

Search results

Number of results: 73
items per page: 25 50 75
Sort by:

Abstract

This paper focuses on mechanical properties of self hardening moulding sands with furfuryl and alkyd binders. Elasticity as a new parameter of moulding sands is investigated. With the use of presented testing equipment, it is possible to determine force kinetics and deformation of moulding sand in real time. The need for this kind of study comes from the modern casting industry. New foundries can be characterized with high intensity of production which is correlated with high level of mechanization and automatization of foundry processes. The increasingly common use of manipulators in production of moulds and cores can lead to generation of new types of flaws, caused by breakage in moulds and cores which could occur during mould assembly. Hence it is required that moulds and cores have high resistance to those kinds of factors, attributing it with the phenomenon of elasticity. The article describes the theoretical basis of this property, presents methods of measuring and continues earlier research.
Go to article

Abstract

One of the purposes of the application of chemically modified inorganic binders is to improve knocking out properties and the related reclamability with previously used in foundry inorganic binder (water glass), which allowing the use of ecological binders for casting nonferrous metals. Good knocking out properties of the sands is directly related to the waste sands reclamability, which is a necessary condition of effective waste management. Reclamation of moulding and core sands is a fundamental and effective way to manage waste on site at the foundry, in accordance with the Environmental Guidelines. Therefore, studies of reclamation of waste moulding and core sands with new types of inorganic binders (developed within the framework of the project) were carried out. These studies allowed to determine the degree of recovery of useful, material, what the reclaimed sand is, and the degree of its use in the production process. The article presents these results of investigation. They are a part of broader research programme executed under the project POIG.01.01.02-00- 015/09 "Advanced materials and technologies".
Go to article

Abstract

This paper presents a new perspective on the issue of reclamation of moulding and core sands. Taking as a premise that the reclamation process must remain on the surface of grains some not separated binding materials rests, it should be chosen the proper moulding sand’s composition that will be least harmful for the reclaim quality. There are two different moulding and core sands taken into examinations. The researches prove that a small correction of their compositions (hardener type) improves the quality of the received reclaims. Carried out in this article studies have shown that such an approach to the problem of reclamation of the moulding and core sands is needed and reasonable.
Go to article

Abstract

The constant growth of foundry modernization, mechanization and automation is followed with growing requirements for the quality and parameters of both moulding and core sands. Due to this changes it is necessary to widen the requirements for the parameters used for their quality evaluation by widening the testing of the moulding and core sands with the measurement of their resistance to mechanical deformation (further called elasticity). Following article covers measurements of this parameter in chosen moulding and core sands with different types of binders. It focuses on the differences in elasticity, bending strength and type of bond destruction (adhesive/cohesive) between different mixtures, and its connection to the applied bonding agent. Moulding and cores sands on which the most focus is placed on are primarily the self-hardening moulding sands with organic and inorganic binders, belonging to the group of universal applications (used as both moulding and core sands) and mixtures used in cold-box technology.
Go to article

Abstract

The last decade has seen growing interest in professional public about applications of porous metallic materials. Porous metals represent a new type of materials with low densities, large specific surface, and novel physical and mechanical properties, characterized by low density and large specific surface. They are very suitable for specific applications due to good combination of physical and mechanical properties such as high specific strength and high energy absorption capability. Since the discovery of metal foams have been developed many methods and techniques of production in liquid, solid and gas phases. Condition for the use of metal foams - advanced materials with unique usability features, are inexpensive ways to manage their production. Mastering of production of metallic foams with defined structure and properties using gravity casting into sand or metallic foundry moulds will contribute to an expansion of the assortment produced in foundries by completely new type of material, which has unique service properties thanks to its structure, and which fulfils the current demanding ecological requirements. The aim of research conducted at the department of metallurgy and foundry of VSB-Technical University Ostrava is to verify the possibilities of production of metallic foams by conventional foundry processes, to study the process conditions and physical and mechanical properties of metal foam produced. Two procedures are used to create porous metal structures: Infiltration of liquid metal into the mold cavity filled with precursors or preforms and two stage investment casting.
Go to article

Abstract

The paper presents the results of the crystallization process of silumin by the TDA thermographic method and the results of the cast microstructure obtained in the sampler TDA-10, that was cooling down in ambient air. The study was conducted for silumin AlSi11 unmodified. The work demonstrated that the use of thermal imaging camera allows for the measurement and recording the solidification process of silumin. Thermal curve was registered with the infrared camera and derivative curve that was calculated on the base of thermal curve have both a very similar shape to adequate them TDA curves obtained from measurements using a thermocouple. Test results by TDA thermographic method enable quantitative analysis of the kinetics of the cooling and solidification process of neareutectic silumin.
Go to article

Abstract

The work presents the results of examinations concerning the influence of various amounts of home scrap additions on the porosity of castings made of MgAl9Zn1 alloy. The fraction of home scrap in the metal charge ranged from 0 to 100%. Castings were pressure cast by means of the hot-chamber pressure die casting machine under the industrial conditions in one of the domestic foundries. Additionally, for the purpose of comparison, the porosity of specimens cut out directly of the MgAl9Zn1 ingot alloy was also determined. The examinations consisted in the qualitative assessment of porosity by means of the optical microscopy and its quantitative determination by the method of weighting specimens in air and in water. It was found during the examination that the porosity of castings decreases with an increase in the home scrap fraction in the metal charge. The qualitative examinations confirmed the beneficial influence of the increased home scrap fraction on the porosity of castings. It was concluded that the reusing of home scrap in a foundry can be a good way of reduction of costs related to the production of pressure castings.
Go to article

Abstract

The work presents the results of examinations concerning the influence of various amounts of home scrap additions on the properties of castings made of MgAl9Zn1 alloy. The fraction of home scrap in the metal charge ranged from 0 to 100%. Castings were pressure cast by means of the hot-chamber pressure die casting machine under the industrial conditions in one of the domestic foundries. The examinations consisted in the determination of the following properties: tensile strength Rm, yield strength Rp0.2, and the unit elongation A5, all being measured during the static tensile test. Also, the hardness measurements were taken by the Brinell method. It was found that the mechanical properties (mainly the strength properties) are being improved up to the home scrap fraction of 50%. Their values were increased by about 30% over this range. Further rise in the home scrap content, however, brought a definite decrease in these properties. The unit elongation A5 exhibited continual decrease with an increase in the home scrap fraction in the metal charge. A large growth of hardness was noticed for the home scrap fraction increasing up to the value of 50%. Further increasing the home scrap percentage, however, did not result in a significant rise of the hardness value any more.
Go to article

Abstract

The work deals with technology Patternless process that combines 3 manufacturing process mold by using rapid prototyping technology, conventional sand formation and 3D milling. It's unconventional technology that has been developed to produce large-sized and heavyduty castings weighing up to several tons. It is used mainly in prototype and small batch production, because eliminating production of models. The work deals with the production of blocks for making molds of gypsum and gypsum drying process technology Thermomold. Into blocks, where were made cavities by milling were casted test castings from AlSi10MgMn alloy by gravity casting. At machining of the mold cavity was varied feed rate of tool of cemented carbide. Evaluated was the surface roughness of test castings, that was to 5 micrometers with feed from 900 to 1300 mm/min. The dimensional accuracy of castings was high at feed rate of 1000 and 1500 mm/min did not exceed 0.025 mm.
Go to article

Abstract

The dimensional accuracy of a final casting of Inconel 738 LC alloy is affected by many aspects. One of them is the choice of method and time of cooling the wax model for precision investment casting. The main objective of this work was to study the initial deformation of the complex shape of a rotor blades casting. Various approaches have been tested for cooling a wax pattern. When wax models are air cooled and without clamping in the jig for cooling, deviations from the ideal shape of the casting are very noticeable (up to 8 mm) and most are in extreme positions of the model. When the blade is cooled in the fixing jig in a water environment, the resulting deviations compared to those of air cooling are significantly larger, sometimes up to 10 mm. This itself does not mean that the final shape of the casting is dimensionally more accurate with the usage of wax models, which have smaller deviations from the ideal position. Another deformation occurs when the shell mould is produced around the wax pattern and further deformations emerge while cooling the blade casting. This paper demonstrates the first steps in describing the complex process of deformations occurring in Inconel alloy blades produced with investment casting technology by comparing results of thermal imagery, simulations in foundry simulation software ProCAST 2010, and measurements from a CNC scanning system using a Carl Zeiss MC 850. Conclusions are so far not groundbreaking, but it seems that deformations of the wax pattern and deformations of the castings do in some cases cancel each other by having opposite directions. Describing the whole process of deformations will help increase the precision of blade castings so that the models at the beginning and the blades in the end are the same.
Go to article

Abstract

The goal of this contribution is summary of physical – chemistry properties of usually used foundry silica and no – silica sands in Czech foundries. With the help of dilatometry analysis theoretical assumptions of influence of grain shape and size on dilatation value of sands were confirmed. Determined was the possibility of dilatometry analysis employment for preparing special (hybrid) sands with lower and/or more linear character of dilatation.
Go to article

Abstract

The paper analyses specific defects of castings produced by semi-solid casting process, especially rheocasting method SEED, which uses mechanical swirling for reaching proper structure in semisolid state with high content of solid fraction. Heat treated alloy AlSi7Mg0.3 was applied for producing an Engine Bracket casting part. For observing structure, metallographic observation by light and SEM microscopy was used. To analyse the process, software ProCAST was used to simulate the movements in shot chamber and filling of the mold.
Go to article

Abstract

Issues connected with high quality casting alloys are important for responsible construction elements working in hard conditions. Traditionally, the quality of aluminium casting alloy refers to such microstructure properties as the presence of inclusions and intermetallic phases or porosity. At present, in most cases, Quality index refers to the level of mechanical properties – especially strength parameters, e.g.: UTS, YS, HB, E (Young’s Modulus), K1c (stress intensity factor). Quality indexes are often presented as a function of density. However, generally it is known, that operating durability of construction elements depends both on the strength and plastic of the material. Therefore, for several years now, in specialist literature, the concept of quality index (QI) was present, combines these two important qualities of construction material. The work presents the results of QI research for casting hypoeutectic silumin type EN AC-42100 (EN AC-AlSi7Mg0.3), depending on different variants of heat treatment, including jet cooling during solution treatment.
Go to article

Abstract

The new investigation method of a permeability of ceramic moulds applied in the investment casting technology, is presented in the paper. Some concepts of performing permeability measurements are shown. Investigations in which the influence of the solid phase fraction in the liquid ceramic moulding sand (LCMS) on a permeability of a multi-layer ceramic mould were performed and discussed. The permeability was estimated during two the most important stages of the technological process: in the first – after wax melting and in the second – after mould annealing. Also an influence of the matrix grain sizes (material for sprinkling) on a ceramic mould permeability was estimated.
Go to article

Abstract

The work is a continuation of research concerning the influence of intensive cooling of permanent mold in order to increase the casting efficiency of aluminium alloys using the multipoint water mist cooling system. The paper presents results of investigation of crystallization process and microstructure of multicomponent synthetic hypereutectic alloy AlSi20CuNiCoMg. The study was conducted for unmodified silumin on the research station allowing the cooling of the special permanent sampler using a program of computer control. Furthermore, the study used a thermal imaging camera to analyze the solidification process of multicomponent alloy. The study demonstrated that the use of mold cooled with water mist stream allows in wide range to form the microstructure of hypereutectic multicomponent silumin. It leads to higher homogeneity of microstructure and refinement of crystallizing phases of casting.
Go to article

Abstract

The work is a continuation of research on the use water mist cooling in order to increase efficiency of die-casting aluminum alloys. The paper presents results of research and analysis process, spraying water and generated a stream of water mist, the effect of the type of nozzle, the nozzle size and shape of the emitting of the water mist on the wall surface of casting die on the microstructure and geometry of water mist stream and cooling efficiency. Tests were used to perform high-speed camera to record video in the visible and infrared camera. Results were used to develop a computerized image analysis and statistical analysis. The study showed that there are statistical relationships between water and air flow and geometry of the nozzle and nozzle emitting a stream of microstructure parameters of water mist and heat the incoming stream. These relationships are described mathematical models that allow you to control the generating of adequate stream of water mist and a further consequence, the cooling efficiency of casting die.
Go to article

Abstract

The article shows the influence of environment requirements on changes in different foundry moulding sands technologies such as cold box, self-hardening moulding sands and green sands. The aim of the article is to show the possibility of using the biodegradable materials as binders (or parts of binders’ compositions) for foundry moulding and core sands. The authors concentrated on the possibility of preparing new binders consisting of typical synthetic resins - commonly used in foundry practice - and biodegradable materials. According to own research it is presumed that using biodegradable materials as a part of new binders’ compositions may cause not only lower toxicity and better ability to reclaim, but may also accelerate the biodegradation rate of used binders. What’s more, using some kinds of biodegradable materials may improve flexibility of moulding sands with polymeric binder. The conducted research was introductory and took into account bending strength and thermal properties of furan moulding sands with biodegradable material (PCL). The research proved that new biodegradable additive did not decrease the tested properties.
Go to article

Abstract

The article contains the results of tests performed under the target project in Hardtop Foundry Charsznica. The objective of the tests and studies was to develop a technology of making high-quality ductile iron castings, combined with effective means of environmental protection. The studies presented in this article related to castings weighing from 1 to 300 kg made from ductile iron of grades 400-15 and 500-7, using two-layer moulds, where the facing and core sand was the sand with an alkaline organic binder, while backing sand was the sand with an inorganic geopolymer binder. A simplified method of sand reclamation was applied with possible reuse of the reclaim as an addition to the backing sand. The cast iron spheroidising treatment and inoculation were selected taking into account the specific conditions of Hardtop Foundry. A pilot batch of castings was made, testing the gating and feeding systems and using exothermic sleeves on risers. The study confirmed the validity of the adopted concept of making ductile iron castings in layer moulds, while maintaining the content of sand with an organic binder at a level of maximum 15%.
Go to article

Abstract

Increasing demands on the utility properties of materials used for castings have led to the production of cast iron with a modified shape of graphite, where the required properties are achieved by a change in graphite shape, its size and layout, and a change in the basic structure of the metal. This paper is focused on the continuous method of producing spheroidal graphite FLOTRET. In the introductory section is summarized the theoretical foundations of the secondary treatment of cast irons, especially the FLOTRET flow method, describes the advantages and disadvantages of the method. The practical part is divided into laboratory and operational tests. Laboratory experiments were conducted on a laboratory-type modifier FLOTRET chamber, which was designed and hydraulically optimized. Experiments were focused on the effects of pressure altitude and amount of modifier on the residual values of magnesium, as conditions for a successful modification. The method was tested in two foundries under operating conditions and in one of them was observed a long-term modification process.
Go to article

Abstract

One of the factors that contribute to the development of foundry moulding technology is environmental protection. The related challenges are effectively satisfied by a new inorganic binder that has been designed for castings made of non-ferrous metal alloys. This article presents in a concise way the test results, showing the ecological character of the new binder at the stage of making moulds, pouring them with metal and cooling of castings, indicating the possibilities for an economic re-use of waste materials formed during practical application of this technology. The results were compared with the results obtained on the sands with organic binders. Studies were carried out under the project POIG.01.01.02-00-015/09 "Advanced materials and technologies."
Go to article

Abstract

The aim of research was creation of a furnace for aluminum alloys smelting “in a liquid bath” in order to reduce metal loss. In the paper, the author demonstrates the results of research on smelting of aluminum alloys in a shaft-reverberatory furnace designed by the author. It has been shown that smelting aluminum alloy in a liquid bath was able to significantly reduce aluminum loss and that shaft-reverberatory design provided high efficiency and productivity along with lower energy costs. Ensuring continuous operation of the liquid bath and superheating chamber, which tapped alloy with the required texture, was achieved by means of the optimal design of partition between them. The optimum section of the connecting channels between the liquid bath of smelting and the superheating chamber has been theoretically substantiated and experimentally confirmed. The author proposed a workable shaft-reverberatory furnace for aluminum alloys smelting, providing solid charge melting in a liquid bath.
Go to article

Abstract

Various examples of the design of cast elements of the equipment used in furnaces for the heat treatment of machine parts are given. Shortcomings in their performance are indicated. Reasons for required stability of equipment are briefly discussed. Elements of equipment illustrate the possibilities of using a charge-carrying pallet with dimensions of 900×600×45 mm as a basis for multi-component technological equipment. Introducing additional elements, such as metal baskets, intermediate pallets or crossbars to the main pallet, it becomes possible to create different configurations of this equipment. The technological equipment presented and discussed here is offered to different plants which heat-treat a wide variety of produced parts. It was found that the reliability and durability of new designed equipment can be checked only during practical use. For large plants dealing with the heat treatment of bulk quantities of parts homogeneous or similar in shape is recommended to use the dedicated tooling.
Go to article

Abstract

For the reason of environmental problems connected with the use of furan binders, attention is increasingly being paid to self-setting mixtures using alkali resols. A resol binder stabilized with KOH, NaOH is hardened by liquid esters with the formation of alkaline salts. The increase of their concentration affects the shortening of the mixture bench life, it also decreases strength, increases abrasive wear to moulds and cores, and results in uneconomical dilution of the reclaim with expensive new base sand. The length of life (bench life) of mixtures plays an important role in the manufacture of huge and voluminous moulds and cores in self-setting mixtures. This study aims at analyzing the function of reactive alkaline salts in the reclaim, monitors the consequences of its thermal exposure on the properties of selfsetting mixtures, and deals with development of methods evaluating its qualities.
Go to article

Abstract

The work is a continuation of research on the use of water mist cooling in order to increase efficiency of die-casting aluminum alloys using multipoint water mist cooling system. The paper presents results of investigation on crystallization process and microstructure of synthetic hypereutectic AlSi20 alloy. Casts were made in permanent mold cooled a with water mist stream. The study was conducted for unmodified AlSi20 alloy and a modified one with phosphorus, titanium and boron on the research station allowing sequential multipoint cooling using a dedicated program of computer control. The study demonstrated that the use of mold cooled with water mist stream and solution heat treatment allows in wide range for the formation of the microstructure of hypereutectic silumins. It leads to the growth of microstructure refinement and spheroidizing of phases in the casting.
Go to article

Abstract

The aging granulate is to activate the blowing agent during the manufacturing process to granulate models can re-expand and shape the model of well-sintered granules, smooth surface and a suitable mechanical strength. The article presents the results of studies which aim was to determine the optimum time for aging pre-foamed granules for pre-selected raw materials. The testing samples were shaped in an autoclave, with constant parameters sintering time and temperature. Samples were made at 30 minute intervals. Models have been subjected to flexural strength and hardness.
Go to article

This page uses 'cookies'. Learn more